产品pin脚焊接流程 Laser Diode Module pin-soldering process

1、先对产品管脚及电线分别加装焊锡First install solder on the pin and wire respectively

注意:产品焊接时佩戴防静电手环;wear anti-static bracelets when soldering;

      焊接时使用的焊接温度320℃。The solderingtemperature is 320℃.

2、使用烙铁将电线上焊接好的焊锡熔化。Use a soldering iron to melt the solder soldered on the wire.


3、熔化的电线焊锡,推移到产品管脚,待管脚焊锡融化后取下烙铁,完成电线的焊接。

The molten wire solder goes to the pin, andthe soldering iron is removed after the pin solder melts to complete thewelding of the wire.

注意:焊接时烙铁轻轻前后移动,加速焊锡的融化;When soldering, moves the soldering iron back andforth gently and accelerate the melting of solder;

焊接时间小于10s。The solderingtime is less than 10s.